Cathy, The biggest difference is that if you are using any fluxes that have an activity level higher than L0 or L1, then you must validate your cleaning process in accordance with Appendix B of J-Std-001C. This is a costly test. So, pricing of product built to class 3 if your facility uses higher activity level fluxes will have a cost impact since this testing is required. Refer to paragraph 4.2 of J-Std-001C. If you have a customer that demands it, they should be willing to pay for the validation testing. If your company wants to advertise that it is capable of class 3 work then you'll have to have the results of the testing done as objective evidence that you are qualified to run product with active fluxes. I've been through the testing. If you need further info, let me know. Good Luck. Bill Kasprzak Moog Inc. Manufacturing Engineering, Electronics > -----Original Message----- > From: Cathy Killen [SMTP:[log in to unmask]] > Sent: Wednesday, February 26, 2003 11:38 AM > To: [log in to unmask] > Subject: [TN] Class 2 to Class 3 Assembly > Importance: High > > Hi, > Just a couple of questions, > > What changes do you make in your process to build a class 3 product when > you > originally build to class 2? > > How do you incorporate this into the pricing of the product? > > > Cathy Killen > Training Officer > Please note: It is your responsibility to scan this E-mail for viruses. > > --------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------