Hi,
I am setting up a QC Station between our
Board Department and the Technicians, who install the PC Boards into
Instruments. I would like nonconformances marked right on the solder
joints with a red marker. If the ink is not removed prior
to the re-work process, will the ink contaminate the Solder
Joints?
I suspect that the surface tension of the solder
will not allow contamination to occur. What do you think?
Thanks,
Ronald G. Currell
Ludlum Measurements,
Inc.
--------------------------------------------------- Technet
Mail List provided as a free service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail
to [log in to unmask]: SET Technet Digest Search the archives of previous posts
at: http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/html/forum.htm for additional information, or contact Keach
Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------