The
board designer makes an SMT stencil layer with apertures for all the SMT
components.
The
designer knows were all the SMT components are, so, while they are designing all
the other
layers, they may as well design a the paste layer.
The
contract manufacturer then reviews that stencil/paste layer and may or may not
make modifications OR
they
may have the stencil house that fabs the stencil make modifications. Such
modifications may
include a reduction or expansion of the aperture size, or, exclusion of
components due to process
constraints.
-Carrie
I would like
your opinion on who would be more suited to
design stencils for SMT PWBs;
the board designer or the
contract-manufacturing engineer.
What do
you do and why?
Donald Kyle C.I.D.+
281-285-7528
---------------------------------------------------
Technet
Mail List provided as a free service by IPC using LISTSERV 1.8e
To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest
Search the archives of
previous posts at: http://listserv.ipc.org/archives
Please visit IPC web
site http://www.ipc.org/html/forum.htm for additional information, or contact
Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------