Dear Technetters, I receive today from a customer a strange report. A few weeks ago, he provided us a batch of bare PCB's for assembly. We first did screen printing with solder paste. Because of some procurement and planning problems, the PCB remained with this solder paste on them for a few days and finally, we washed them and gave them back (unpopulated) to our customer. He (and we) noticed that there remained some grey areas on the pads, corresponding to the surface where solder paste was deposited. The PCB manufacturer was consulted, he sent a PCB for analysis, and the answer came: "There remains solder paste residues on the gold, which can be eliminated with desoldering braiding However, the chemical gold layer has been partially desolved, and thus, the Nickel layer is no longer garantied reliable" I accept that cleaning could leave some paste residues on the pads (trapped into the uneven surface of the gold layer) But :we use a no clean solder paste, and we had never heard that the flux could destroy the gold layer !! Who met such a problem or has a technical answer ? Many thanks for your help ME Magnin QA Manager FIRSTEC SA Rue du Grand Pré 70 CH 1211 Genève 2 Tél. : +41(0)22 918 36 85 Fax : +41(0)22 918 36 93 mailto:[log in to unmask] http://www.firstec.ch --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------