Carrie, This parameter has always been at this temperature for as long as I can remember. Basically, the general guideline that I follow is that I leave my pot set at this temperature and my conveyor speed at 4.0 feet per minute. I adjust my preheat temps so that I see top side board temps of 90 - 100 C just prior to the wave. This is the point where flux activity is maximized. Profiles that I have run have indicated that I achieve 3 to 6 second topside joint exposure above the liquidus temp of the 63/37. This gives me great top side wetting on thru hole components without causing reflow of existing SMD joints. That is why 260C is a good temp for the typical PC usual typical PC board. That's why I use this temperature and conveyor setting. Then all is needed is adjustment of the preheat parameters. I did have one instance where a PCB vendor recommended a 220C solder temperature to prevent a delam from occurring at a flex junction. That's what we did. We were able to do this because the board was on the thin side (.045"). But we did have to schedule these boards for specific time periods so the solder pot could stabilize at 220C. Changing the temperature of 2000 lbs. worth of solder takes time. Hence another reason for the 260C, it just seems to be a good universal temperature to keep this massive amount of metal set for good general soldering. I would have to think that lower pot temps would affect the quality of topside fillets on some of my backplane boards. I would have to offset the lower pot temperature with higher preheat temps or slower conveyor speeds. I think that doing this would reduce the flux activity. So the benefits of lower pot temps would have to be quantified before I start messing with the 260C setting. Most component specs, (that I can recall), specify 260C as the exposure temperature. (e.g. 260C for 10 sec.) This would be another reason for the 260C temp selection. Should be interesting to see if anyone does something different and why. Bill Kasprzak Moog Inc. Manufacturing Engineering, Electronics > -----Original Message----- > From: Morse, Carrie [SMTP:[log in to unmask]] > Sent: Friday, January 10, 2003 3:15 PM > To: [log in to unmask] > Subject: [TN] Wave Temperature > > As I sit here on a Friday afternoon with little time to start thinking > about questions that would be great for a "PCB Assembly Trivial Pursuit" > game, I thought of something. > > At what temperature does everyone run their Sn63Pb37 wave machine....and > Why? > > We run ours at 260C, but, don't know why. We started to get into the > discussion as to why, and, some of the reasons were: 1) That's what was > recommended, 2)It's hot enough to burn off the flux, 3)It reduces surface > tension. > > Can someone enlighten us? > > Thanks, > Carrie > > --------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------