Thanks Susan, We will check this tomorrow! I'll let everyone know the out come! Right now we are pulling our hair out here! As a alternate supervisor of this shop and have never had to deal with this and uppers, wanting production. I'm just pull things out of the air, trying to figure this out. Thanks for all the help from everyone! Randy On Wed, 8 Jan 2003 16:13:24 EST, [log in to unmask] wrote: >Randy >Are you seeing these "spots" in the as polished condition prior to >microetching the mount" ? If you are, it can usually mean that there is >contamination there that has been plated around. That would help in trying >to find out what it is. > >Another thing you can do with your process is to take your panels through >drill and etchback processing and then instead of going through the >electroless line - put them through the oxide line. The metallic areas - >ends of inner layers - should all darken with the oxide. If there is resin >or non-metallic areas on the ends of the inner layers they won't be coated >with the oxide. > >The fact that there is an indentation in the inner layer where the "ball" is >located really is a concern when trying to troubleshoot what is happening. >If the glass bundles are laying on top the inner layer and are being plated >around, I wouldn't expect to see the indentation - almost as though they have >been forced into the end of the inner layer. > >Susan Mansilla >Robisan Lab > ><font size="2">---------------------------------------------------<br> >Technet Mail List provided as a free service by IPC using LISTSERV 1.8e<br> >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet<br> >To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)<br> >To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest<br> >Search the archives of previous posts at: http://listserv.ipc.org/archives<br> >Please visit IPC web site http://www.ipc.org/html/forum.htm for additional >information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315<br> >-----------------------------------------------------<br></font> > <font size="2">---------------------------------------------------<br> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e<br> To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet<br> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)<br> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest<br> Search the archives of previous posts at: http://listserv.ipc.org/archives<br> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315<br> -----------------------------------------------------<br></font>