Pankaj, I suppose you're looking for data on original build, but for BGA rework we generally use stencils with the following dimensions. Pitch Stencil Thickness Aperture Diameter .039"(1.00 mm) .004"(0.102 mm) .020"(0.508 mm) .050"(1.27 mm) .006"(0.152 mm) .025"(0.635 mm) We have exception to these sizes, but use them as a starting point. I have some additional info at: http://www.circuittechctr.com/products/201-3120.htm. Jeff Ferry CEO Circuit Technology Center, Inc. http://www.circuittechctr.com [log in to unmask] 978-374-5000 x14 Sign up for our Free E-mail Newsletter at: http://www.circuitnet.com/subscribe.htm -----Original Message----- From: Karnwal, Pankaj [mailto:[log in to unmask]] Sent: Wednesday, December 18, 2002 11:17 PM To: [log in to unmask] Subject: [TN] BGA paste deposit Hello Technet I want know that how much solderpaste deposit required for reliable BGA soldering with respect to the pitch and the pad size. Is that the 120% of the pad in case of less than 1mm pitch ( Micro BGA ) With regards Pankaj Karnwal QualityAssurance BESL A-4,Sec-5 NOIDA,201301,INDIA e mail : <mailto:[log in to unmask]> Barco,innovators in image processing --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------