Hi, We are using hot air not only to remove, but solder the component back onto the pad as well. However, it is very much depending upon operator's skill. Not all operators can do that well. Poh --- Kathy Kuhlow <[log in to unmask]> wrote: > The hot air technique might work well for the 20mil pitch device if > it has enough mass. I have found with 0603 and 0402 hot air reflow > is only good at blowing the part off the PCB. I would suggest a > tweezer soldering iron for those parts. > > Kathy > > > >>> [log in to unmask] 11/27/02 03:48PM >>> > Can anyone recommend good soldering technique for > hand assembly of 20mil pitch devices and 0603, 0402 > SMT chips? We are looking at doing some protoype > assembly on some fairly dense (and small) pcbs. We > were thinking of using solderpaste and one of those > portable solder pens with a hot air tip ie. Weller > Portasol. Has anyone had success using this > technique? > Thanks > Ron. > > --------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV > 1.8e > To unsubscribe, send a message to [log in to unmask] with following > text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: > http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for > additional > information, or contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ----------------------------------------------------- > > --------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV > 1.8e > To unsubscribe, send a message to [log in to unmask] with following > text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: > http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for > additional > information, or contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------