Jean-Francois, Yes, it sounds like flux residue. However, this is an opinion. To be certain, the residues should be analyzed. There are several organizations with the capability to perform the analysis. Reliability and the effects of leaving the residue in place or the effects of removal processes are another issue beyond the scope of this response. Don Vischulis -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Bissonnette, Jean-Francois Sent: Tuesday, November 12, 2002 8:58 AM To: [log in to unmask] Subject: [TN] Flux emtrapment? I have spoted white residues under header Socket strips. It looks like some kind of crust and some times the residues observed looked like yellow translucent crystals. Can this be entraped flux? I beleive so, but need to have opinion from experts to conform. Thanks in advance. Jean-François Bissonnette Vérificateur, Contrôle de la Qualité Électronique Produits et Procédés Vapor Rail Inc. 10655 Henri-Bourassa O. St-Laurent, Qc H4S 1A1 (514) 335-4200 x2021 (514) 335-4231 fax WABTEC CORPORATION CONFIDENTIALITY NOTE The content contained in this e-mail transmission is legally privileged and confidential information intended only for the use of the individual or entity named herein. If the reader of this transmission is not the intended recipient, you are hereby notified that any dissemination, distribution, or copying of this transmission is strictly prohibited. --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------