Werner,
Thankfully, I don't have any pictures of that problem, but I may take some scrap/obsoleted/ or otherwise trash parts and soak them to produce some pictures. But in the mean time, here's a pretty good link that does have some SEM images of "Pop-corning"...good technical paper too.
http://rel.intersil.com/docs/rel/98_pem_consortium/98_pem_consortium.pdf
-Steve Gregory-
Hi 'Netters,
Could any of share some good pictures of a 'popcorned' component and a
component with delaminated die. I would of course give full credit as to
source.
Thanks,
Werner Engelmaier
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------