I wouldn't worry about it. It does not sound like you are relying on the solder fill to do anything. So, cracking of at the interface of the solder to the gold would not matter. Am I missing something here? > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez > Sent: Friday, November 01, 2002 8:23 AM > To: [log in to unmask] > Subject: [TN] Plating Au over Cu > > > Fellow TechNetters, > > Can you please share your concern with plating hard gold, > 25 micro inches, on fingers of a PCB over > an area adjacent to PTH's where some unplugged via exhibit > SnPb. I guess > my main concern is Au/SnPb. > > Victor G. Hernandez > > --------------------------------------------------- > Technet Mail List provided as a free service by IPC using > LISTSERV 1.8e To unsubscribe, send a message to > [log in to unmask] with following text in the BODY (NOT the > subject field): SIGNOFF Technet To temporarily halt or > (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE > mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest Search the archives of > previous posts at: http://listserv.ipc.org/archives Please > visit IPC web site http://www.ipc.org/html/forum.htm for > additional information, or contact Keach Sasamori at > [log in to unmask] or 847-509-9700 ext.5315 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------