I wasn't aware that this technology had reached the point where laser trimming would be valuable, interesting. As I am sure you know resistor trimming with feedback is standard stuff in hybrid thick film, I am not sure this would translate to organic substrates though. CO2 lasers would likely cut into if not through the board, I think even a Yag laser would have trouble differentiating between the ink and the board and less powerful laser technologies would be very slow and probably would require re-configuration to be a trimmer . Be interested to see what other (more informed) 'netters have to say. Regards Mike Fenner Applications Engineer, European Operations Indium Corporation T: + 44 1908 580 400 M: + 44 7810 526 317 F: + 44 1908 580 411 E: [log in to unmask] W: www.indium.com Leadfree: www.Pb-Free.com -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of David Sent: Monday, November 18, 2002 2:32 PM To: [log in to unmask] Subject: [TN] Laser Trimming equipment for resistive ink Hello Fellow TechNetters, I am looking for any recommendation to the above equipment to work with resistive ink, also called buried resistors, in PCB. Could such an equipment perform resistance test and provide feedback loop for laser trim? Would also aprreciate any information or papers relating to the resistive ink. Thanks for the help. Best regards, David. --- Outgoing mail is certified Virus Free. Checked by AVG anti-virus system (http://www.grisoft.com). Version: 6.0.394 / Virus Database: 224 - Release Date: 10/3/02 --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------