The 0.25" is still much wider than the edges that need to be coating-free on some of our boards. The ideal solution would be to have a tape just as wide as this free edges. Frank On Tue, 12 Nov 2002 11:06:53 -0500, "Phil Nutting" <[log in to unmask]> said: > Frank, > > Try http://www.humiseal.com/tape.htm for HumiTape. Pick HT-600 for > anti-static, sizes from 0.25" to 2" wide, dots also available. > > Phil Nutting > > -----Original Message----- > From: circuitguy [mailto:[log in to unmask]] > Sent: Tuesday, November 12, 2002 10:52 AM > To: [log in to unmask] > Subject: [TN] Masking tape for conformal coating > > > Hello Technet, > > Does anyone know a supplier for a 3 mm wide masking tape to be used at > conformal coating. The standard tape that I use is about 8 mm and not > always suitable. > > Frank Agillo-- > http://fastmail.fm - Choose from over 50 domains or use your own > > --------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: > http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for > additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > ----------------------------------------------------- > -- http://fastmail.fm - Send your email first class --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------