How high is the setting? Our tinning pots are typically sett at 500degF. The surface does oxidize quickly after the dross is skimmed off but is usually "gold" in color turning grey. Black dross would indicate something other than just normal oxidation, although a lot of flux on the wire might account for some of this. Are you tinning silver plated wire? I have seen an almost black film accumulate from the silver oxides. Charles Caswell The Big Kahuna PCB, Frontier Electronic Systems -----Original Message----- From: Hogg, Blair K. [mailto:[log in to unmask]] Sent: Wednesday, October 23, 2002 4:27 PM To: [log in to unmask] Subject: [TN] Dross on Solder Pot Hello Technetters, I'll readily admit that I'm not an expert on solder, and something has been bothering me lately here at the shop, so I'll see what insight the forum can yield. We have a small solder pot used for tinning wires in our harness area. Periodically as I walk by this pot I notice fairly thick black dross covering the surface of the solder. This gets wiped away before they tin wires, but lately I've noticed it turns brownish fairly quickly after wiping off the dross from the surface. What can be the typical causes of this? Could the pot be too hot? Could the pot be contaminated (e.g. with copper)? Could it be contaminated because it's too hot? I'm suggesting heat here because they run this pot at a fairly high setting, I'm not sure why. Thanks, Blair Hogg QA Manager GAI-Tronics --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------