1/2 oz. copper is twice as thick as 1/4 oz. copper, and half as thick as 1 oz. copper : ) Unless of course there is pattern plating involved : ( JaMi Smith ----- Original Message ----- From: "Graham Collins" <[log in to unmask]> To: <[log in to unmask]> Sent: Wednesday, October 16, 2002 12:00 PM Subject: [TN] how thick is ½ ounce copper Hi Technet! A simple question for the fab gurus out there - but one over the head of this assembly grunt. How thick is ½ ounce copper? regards, Graham Collins Process Engineer, Northrop Grumman Canada Corporation Halifax (902) 873-2000 ext 6215 ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------