Soldering directly to brass can lead to "dezincification", an embrittling reaction between the tin in the solder and the zinc in the brass. Good practise is to plate the brass with an immunising layer to prevent this. Your brass bits supplier should be familiar with this and have a standard process on his books. Regards Mike Fenner Applications Engineer, European Operations Indium Corporation T: + 44 1908 580 400 M: + 44 7810 526 317 F: + 44 1908 580 411 E: [log in to unmask] W: www.indium.com Leadfree: www.Pb-Free.com -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Phil Nutting Sent: Thursday, October 03, 2002 8:23 PM To: [log in to unmask] Subject: [TN] soldering brass to copper I vaguely remember something about soldering brass in some recent posts. We are looking at some cooling parts that may require soldering brass to copper. My experience says that this is a non-problem. The posts that I remember said something about tin and crystallization. Am I mixing two different thoughts here? Phil Nutting Manufacturing Engineer Kaiser Systems, Inc. voice: 978-922-9300 e-mail: [log in to unmask] ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------