Reapplication of dissipative floor finish depends upon the traffic. As the layer wears the RTT resistance point-to-point, measured in ohms, will increase. Taking this measurement should be a regular part of a company's ESD control plan compliance verification plan. As the floor finish wears, it will come closer to an insulative resistance range. Tracking this over a period of time will allow the user to define a maintenance schedule that will optimize performance while minimizing material and labor costs. The current issue of EE Evaluation Engineering has an article regarding reducing ESD floor maintenance costs at http://www.evaluationengineering.com/archive/articles/1002esd.htm Gene Felder [log in to unmask] -----Original Message----- From: Phil Nutting [SMTP:[log in to unmask]] Sent: Thursday, October 31, 2002 8:17 AM To: [log in to unmask] Subject: [TN] ESD floor wax Good morning, We are looking at some new assembly space an we have an opportunity to make the floor whatever we want. Three options, ESD tiles, ESD carpet or ESD wax. Regarding the ESD wax, does anyone have opinions about 4500 Staticide Gold or 4600 Staticide Ultra available from Techni-Tool? Is the 24 month "wearability" a real number? If you prefer, offline comments gladly accepted. Thanks in advance, Phil Nutting --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------