At risk of repeating myself, and others... The problem you are having is because the etch is accelerated by the galvanic action of the Gold/Copper galvanic cell that forms, and jacks the etch speed WAY up... This does not happen nearly as much with Tin/Copper because they are similar in electronegativity (a chemists way of saying they both give up their electrons with a similar voltage applied) ....and also because the Tin forms a nicely non-conductive oxide on the surface, which is a blanket to the electron exchange. ONLY way to deal with this is to cut exposure time in the ammoniacal etcher. And this is difficult to predict/preset, as the etch speed of ammonia etchants can vary a whole lot, because the etch ingredients and parameters are mostly uncontrolled, except of course for the metal content. This etchant makes me crazy, and I predict the industry will see a day when both pH control, and air control (via ORP) will be the norm. Rudy Sedlak RD Chemical Company --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------