Bill Brooks
--------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------------Original Message-----
From: Brooks,Bill [mailto:[log in to unmask]]
Sent: Tuesday, October 22, 2002 12:08 PM
To: [log in to unmask]
Subject: Re: [TN] Solder UNDER Soldermask Accept/Reject Criteria?The Print did not specify SMOBC. But it also didn't specify SOS (Soldermask over solder) either! The implication is that the order of the notes IMPLIES that we want soldermask after the solder coating process. Don't all PCB vendors know that the solder under the soldermask will reflow, wrinkle and damage the soldermask in assembly? If we have soldermask on a thru hole technology board.... we are going to wave solder the board. Why would a vendor interpret the drawing in such a way as to compromise the performance of the board? I can't believe this is still happening in 2002. I thought we learned our lesson back in 1980.....the first time I ever saw anyone DO that...Doesn't IPC have a spec that tells us not to do it that way?Bill Brooks
-----Original Message-----Hi Bill!
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Tuesday, October 22, 2002 11:44 AM
To: [log in to unmask]
Subject: Re: [TN] Solder UNDER Soldermask Accept/Reject Criteria?
Was that called out on the fab drawing? I've ran across a few boards here that still call that out on the drawing, and TRY and get that changed before the boards are fabbed...most of the time I've been lucky, but there's been a few that slipped by me.
Bottomline, if it's called out on the drawing, you don't have much recourse...
-Steve Gregory-
Anyone aware of a spec that sets the accept/reject criteria for boards that
come in with solder UNDER the soldermask? Is this actually done as a
legitimate practice? WHY would a vendor make the boards this way? Shouldn't
we be making all boards to be SMOBC when there is a soldermask?
Bill Brooks
--------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------