The choice of stripper will always
depend upon what you are trying to remove, and what the substrate is susceptible
to damage by. I agree with Brian that DCM gets an unnecessarily bad press,
but legislation is legislation. Questionable science seems to hit this
industry as much as any other.
However, DMSO
(Dimethylsulfoxide) has been proffered as a more environmentally acceptable and
safe to use solvent, with similar solvency properties to DCM, but has far fewer
legal H&S requirements. That is if you can get over the name of the
corporation that supplies it ;-) ...
Hope of some use.
Best Regards,
Phil
Please note that Concoat has recently acquired the former Multicore SPCID
business. For more information, please visit our new web site
www.concoatsystems.com
Concoat Ltd
Alasan House, Albany Park,
Camberley, Surrey,
GU16 7PH
Tel: +44 (0) 1276 691100
Fax: +44 (0) 1276
691227
----- Original Message -----
Sent: Tuesday, September 03, 2002 8:13
PM
Subject: [TN] PAINT STRIPPERS
Deer Technetters:
Does anyone have a recommendation for
a methylene chloride-free paint
stripper?
Thanks in advance...
Jim
Marsico
Senior Engineer
Production Engineering
EDO Electronics
Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
---------------------------------------------------------------------------------
Technet
Mail List provided as a free service by IPC using LISTSERV 1.8e
To
unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt
or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or
(MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet
Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please
visit IPC web site http://www.ipc.org/html/forum.htm
for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------