Technet, We are having problems replacing 35mm BGA, 1.27mm pitch on a OK industry BGA rework station. The resulting X-ray revealed a solder bridge at one corner. There was some warpage on the BGA but not significant. PCB was reasonably flat. Thermal profiling was done to ensure all temp. were optimum. I did notice the BGA balls collapsing quite a bit (at least half of the ball height) after rework. Anyone has suggestion on how to minimize the chance of bridging? Is it common for BGA of this size? We don't have the capability to paste the board for BGA rework. Rgds, Peter --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------