The average for my pot over the last 8 months is: Tin - 63.146% Lead - Remaining % Sb - .00955% Cu - .100% Au - .00186% Al - <.001% Cd - <.001% Zn - < .001% Ni - <.001% Gary Camac "McCall,Doug" wrote: > Techies, > > I am interested in finding out what the solder analysis figures > should be from the sample taken from the flow solder bath sample. > > Percentages of the following elements would be useful: - > Tin, lead, antimony, copper, zinc, iron, nickel, bismuth, cadmium, > Silver, gold, arsenic, aluminium etc. > > We are using 63 / 37 bar solder into the machine. > > Also any mil-spec equivalents would be useful. > > Thanks in anticipation, > > Regards, > > Doug McCall > PCB Manufacturing Engineer - Eastbourne > BOC EDWARDS > Marshall Road, > Eastbourne, > East Sussex, > BN22 9BA UK > Tel: +44 (0) 1323 501 147 > Fax +44 (0) 1323 509 824 > mailto [log in to unmask] > > BOC Edwards is a part of BOC Limited > Registered Office: Chertsey Road, Windlesham, Surrey GU20 6HJ > Number 337663-English Register > Ultimate holding company: The BOC Group plc > > _____________________________________________________________________ > This e-mail has been scanned for viruses by the WorldCom Internet Managed Scanning Service - powered by MessageLabs. For further information visit http://www.worldcom.com > > --------------------------------------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------