Bev Ethylene glycol, as a monomer, its dimer and trimer should not be confused with polyethylene glycols (PEGs). The latter (Carbowax), with MWs over about 300 and especially over 1000, will bond terribly with epoxies at soldering temperatures, causing distinct SIR losses. You don't say whether the EG has been subjected to high temperatures or is a room-temperature contaminant. If the latter and it is pure (or a pure water/EG mix), I would say a simple but thorough DI water wash and rinse will be sufficient. If it is not pure, (e.g. the stabilisers in anti-freeze, which may be amines) look to the other contaminants, as well. If the assembly has passed the Tg of the epoxy since contamination, the "searching" qualities of the EG may mean some penetration and a long hot soak may be needed to leach out the absorbed product. I would not add anything to the water. EG itself has surfactant qualities. A saponifier will not react with a diol so would not do anything. Ideally, an SIR test after cleaning would be good confirmation but, at the least, a thorough electrical testing should be done, preferably in a climatic chamber. Brian Bev Christian wrote: > Technettters, > Say you had a populated, expensive circuit pack that had been contaminated > with ethylene glycol. Would you chuck it or clean it? I seem to recall > that before I entered the industry that there was a time when some type of > glycol was used on making printed circuit boards(?). The reason I mention > this, is if this were true, can glycols chemically bond at room temperature > to PCBs by more than hydrogen bonding, to the point where a water wash, > saponified or not, would not be able to remove the glycol. I am assuming > there are no standoff issues. > > regards, > Bev Christian > Research in Motion > > --------------------------------------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > --------------------------------------------------------------------------------- > > > --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------