Based on Temperature cardboard is not a good idea, even lined will cause a fire. New paint buckets or regular gal water buckets. Not sure how much solder your talking about. I had to empty an electrovert couple years ago and that filled several galv water buckets. Have to go slow the solder will splash. Be sure to wear an OBA or other breathing apparatus, and be sure the filter is for LEAD, NOT DUST. Also EYE, hand, arm, shoe and leg protection of some sort. Randy ----- Original Message ----- From: Steve Gregory To: [log in to unmask] Sent: Friday, August 23, 2002 8:46 AM Subject: [TN] Emptying wave solder pot Hi All! In a couple of weeks, I'm going to have to empty the wave solder pot on our Treiber. In the past, I remember round cardboard containers being used to put the solder in after ladling it from the pot. Does anybody know where I can get those? Thanks! -Steve Gregory- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------