All
I am looking for a small piece of equipment that can be used to put a constant cyclic strain on a solder joint, otherwise known a fatique testing. I would like the equipmet ot withstand operating temperatures up to 175oC. If any one knows of a supplier of such a piece of equipment or has one for sale, let me know.
Phil Hinton