Hi, Joe, I, too, am interested in any comments on the AAT machines, as I am looking to buy one of their small cleaners for our prototype shop. My information so far is that they're reliable, easy to use and require little maintainance apart from filter changes. That's sales pitch, though, of course. Haven't experienced the real thing yet. Peter "Kane, Joseph" <[log in to unmask]> 21/08/2002 05:56 AM Sent by: TechNet <[log in to unmask]> Please respond to "TechNet E-Mail Forum."; Please respond to "Kane, Joseph" To: [log in to unmask] cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group) Subject: [TN] In-Line Aqueous Cleaners We're in the process of choosing a source for a new cleaner. We use RMA today with batch semi-aqueous systems, and we're buying a conveyorized aqueous system so that we can begin to evaluate water soluble fluxes. Our product is primarily military/high-rel, with some surface mount components spaced very close (e.g. LCC's with 2 mil clearance). We've narrowed it down to Technical Devices, Trek, Electrovert (Speedline), and Austin American Technology. They all look like good machines, and performed well in our evaluations. Anyone care to comment about experiences with their equipment, in the areas of performance, maintainability, recurring costs, reliability, service, availability of parts, etc? Testimonials are welcome and valuable, but if you have a horror story, I'd sure like to hear it, and you can respond to me off-line if you'd be more comfortable. Joe Kane BAE SYSTEMS Controls Johnson City, NY --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- [This e-mail is confidential and may also be privileged. If you are not the intended recipient, please delete it and notify us immediately; you should not copy or use it for any purpose, nor disclose its contents to any other person. Thank you.] --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------