[log in to unmask]">
Dear Jana:
Exposed bare copper (or basis metal) is allowed
on electronic assemblies per IPC-A-610C Paragraph 6.5.2. Hope this helps.
Gregg A. Owens
Executive Director
Manufacturing Technology
Training Center, Inc.
10427 San Sevaine Way, Suite
"I"
Mira Loma, CA 91752
Phone: (909) 360-1324
Fax: (909) 360-1346
Website: www.mttc-inc.com
-----Original Message-----
From: TechNet
[mailto:[log in to unmask]] On Behalf Of Jana
Carraway
Sent: Wednesday, July 17, 2002
3:48 PM
To: [log in to unmask]
Subject: [TN] Exposed copper in
assemblies
Happy Summer Greetings to
all...and hopefully you are all unable to actually enjoy the weather because
you're working!
Is there current or
recently current literature available on the evils, or not so evils, of exposed
copper in assemblies? Any references to sources on this topic would be
greatly appreciated.
Thank You,
Jana Carraway
Micro Systems
Engineering, Inc.