Kathy , We do many impedance boards and the vast majority of our customers want to see results traceable to the panels any board came from. We add impedance coupons representative of the board design ( 2 per production panel ) and serialize them to the boards in that panel. We test and supply data from these coupons in a report . The coupons are in some cases also supplied to the customer but in most cases are held for a period of time in case retest is required. Regards Paul Greene , Rexcan Circuits Kathy Bergman wrote: > Hello and Happy Independence Day (almost): > > We manufacture PCB's. We are just beginning to do TDR testing in house. > Is there anything in the IPC standards that I can use as a guide in > determining what percentage of a lot is a representative sample of the > results? Would you, as customers, require to see a 100% verification (a > value for each board), or would you be comfortable with a representative > lot report. I am writing a work instruction, and TDR Certificate for the > process. > > Your help is appreciated. > K. Bergman > Quality Manager > ICPC Etched Circuits > > --------------------------------------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------