No Glass Fabric, Base, Epoxy-Resin Binder GEE - Glass Fabric Base, Epoxy Resin, Electrical Grade (G-10) GEB - Glass Fabric Base, Epoxy-Resin, High Temperature Electrical Grade (G-11) GEE-F - Glass Fabric Base, Epoxy-Resin, Flame Resistant, Electrical Grade (FR-4) GEB-F - Glass Fabric Base, Epoxy-Resin, High Temperature, Flame Resistant, Electrical Grade (FR-5) Dave Fish ----- Original Message ----- From: "Marsico, James" <[log in to unmask]> To: <[log in to unmask]> Sent: Tuesday, July 23, 2002 6:13 AM Subject: [TN] LAMINATE MATERIAL > Quick question... is type GEE (MIL-I-24768/2) the same as FR-4? > > Jim Marsico > Senior Engineer > Production Engineering > EDO Electronics Systems Group > [log in to unmask] <mailto:[log in to unmask]> > 631-595-5879 > > -------------------------------------------------------------------------- ------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > -------------------------------------------------------------------------- ------- > --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------