Adam Another concern is that the should be inverted half way through the etching process. Otherwise the circuits will effectively move vertically upwards because the lower edge undercuts significantly faster than the upper edge. Don Vischulis -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Adam Seychell Sent: Monday, July 22, 2002 9:49 PM To: [log in to unmask] Subject: [TN] immersion etching Does anyone etch boards with a simple immersion dip in agitated solution ? I realize spray etching is the norm, but I was hoping to get some info on immersion etching and avoid some of the problems of relatively complex spray equipment. (since etching rate is not a prime concern for us). After some experimentation I found agitation with large amounts of fine bubbles works the best. About 80 L/min (3 cfm) of air evenly distributed over a tank bottom area of 500x300mm (20"x12"). Porous rubber hose seems to produce finer bubbles and better distribution than a few holes drilled into a length of PVC piping. I'd be interested learning more about what is out there in the world of etching. regards, Adam Seychell ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------