Thanks you very much for your help. Regards, Ramon > -----Original Message----- > From: Steve Gregory [SMTP:[log in to unmask]] > Sent: Thursday, June 27, 2002 2:03 PM > To: [log in to unmask] > Subject: Re: [TN] Masking Caps > > Ramon, > > Check with a company called Caplugs, I use them for supplying me masking > boots prior to conformal coating. They have static dissipative material > that they can make them out of. Go to: > > http://www.caplugs.com/ > > What I do is send them a board that I have masked with tape to show them > what I'm trying to mask, then they send me some samples of the boots > they've selected to be sure that they will work, then I'll order them. > Most of them that I have used are stock items. Their standard turn is two > weeks... > > -Steve Gregory- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------