Hi Bev, David & All T's, While I concur with David's "big enough" statement, I also assume he does not include in "if you can detect it, it is too big!" cross-sectioning. On the other hand, Bev writes "Shades of voids in BGAs... How big of a crack in thermally cycled solder joints is too big of a crack?" Cracks in thermally cycled solder joints have nothing to do with voids; therefore why "Shades of voids in BGAs...". Solder exhibits micro-voids [having nothing to do with voids] at grain boundary intersections after about 25 to 30% of the fatigue life having been consumed, and micro-cracks along grain boundaries after about 40%. That means about 60% of life is still available when 'observable' micro-cracks are present. David then says: "A better question would be how do you distinguish between a crack and a void?" That one is easy, voids a roughly spherical, cracks are fractures. Werner Engelmaier Engelmaier Associates, L.C. Electronic Packaging, Interconnection and Reliability Consulting 7 Jasmine Run Ormond Beach, FL 32174 USA Phone: 386-437-8747, Fax: 386-437-8737 E-mail: [log in to unmask], Website: www.engelmaier.com --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------