Hi Guy! Steve and I were on the same page for SERA for surface finish analysis and using other techniques such as CVS, titration, AA, etc. for plating bath chemical parameter analysis. The SERA system can be setup in such a manner as to "drill" through some of the surface finishes to characterize the intermetallic species beneath a plated surface. My personal preference is to use XRF to characterize the plating thickness (using good calibration standards) and use SERA to characterize the plating surface characteristics. But there are a number of SERA users who are very successfully using the "drill" method on intermetallic characterization. The Rockwell Collins experience with immersion tin is that there are some immersion tin chemistries which perform well and some which perform poorly in terms of multiple reflow robustness. It is very important to characterize an immersion tin surface finish in terms of your own manufacturing process expectations and not just run a standard "bake" test. You would be amazed at how many adhesive cure bakes can creep into an assembly process flow in addition to the number of passes through a reflow oven. Dave Hillman Rockwell Collins [log in to unmask] "Guy Ramsey" <[log in to unmask]> on 06/21/2002 06:25:14 AM To: "TechNet E-Mail Forum." <[log in to unmask]>, <[log in to unmask]> cc: Subject: RE: [TN] Immersion Tin I think you're correct; Steve was thinking of a different tool. Two reflows then wave . . . HUMMM I can see two reflows then selective . . . AHHH But Dave, Ioan seemed to be having trouble after reflow. If the problem is formation of unprotected IM, would in-coming SERA predict the process problem? SERA attempts to measure oxide species and thickness not the actual tin thickness. More importantly, and based on your experience, would you expect IT to perform well in a multiple reflow process sequence? Wasn't this one of the big complaints about OSP? > -----Original Message----- > From: TechNet [mailto:[log in to unmask]]On Behalf Of Dave Hillman > Sent: Thursday, June 20, 2002 5:03 PM > To: [log in to unmask] > Subject: Re: [TN] Immersion Tin > > > Hi Steve! Sorry but I have to disagree with you. SERA is a tool which can > be used to extensively characterize a variety of surface finishes on > printed wiring boards and any other surface that can be tested within the > SERA equipment configuration limitations. I believe you may be confusing > SERA with ECI's CVS instrumentation. The CVS equipment measures certain > plating bath chemistry parameters. The SERA equipment is similar to Auger > spectroscopy in analyzing surface finishes. Rockwell Collins has been > successfully using SERA since 1991 in a wide variety of applications (keep > in mind I'm a bit biased on this subject - Rockwell Collins was heavily > involved in the development of the SERA equipment). > > Dave Hillman > Rockwell Collins > [log in to unmask] > > > > > Steve Kelly <[log in to unmask]>@ipc.org> on 06/19/2002 01:13:02 PM > > Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; > Please respond > to Steve Kelly <[log in to unmask]> > > Sent by: TechNet <[log in to unmask]> > > > To: [log in to unmask] > cc: > > Subject: Re: [TN] Immersion Tin > > > SERA will not help you - it is only a tool to measure tin /copper > concentrations . We have been running immersion tin for 5 years with no > issues but only one thermal excursion is allowed. The tin forms a > copper/tin intermetallic after thermal. We even silkscreen before tin to > eliminate this bake cycle. Regards Steve > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan > Sent: Wednesday, June 19, 2002 12:07 PM > To: [log in to unmask] > Subject: Re: [TN] Immersion Tin > > Hi Tony, > > we experienced poor wave soldering after 2 reflows with immersion tin. > So, > please give me a few hints on SERA. Is it a test that the board house > will > do, or it has to be at our incoming? Does it imply additional charges? > Where > can I read more? > > Thanks, > Ioan > --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------