The whole notion of "no-clean" fluxes is that you do not need to clean them: it's as simple as that. IPA is not, in any case, a good solvent for flux residues. The combination you state will almost inevitably produce the results you observe. If you think you need to clean after hand soldering, the first question to ask is, "Why clean?" ( http://www.protonique.com/plcom/files/whycl.htm ). If you then decide you must clean, you must then examine the flux and cleaning chemistry and processes as an ensemble and not as four separate items, to put the best chances on your side. Brian "Karnwal, Pankaj" wrote: > > Dear all > > Some time we are facing a problem after hand soldering . > > After wave solder soldering we puts some components like transformer, > connectors etc. ( Due to shortage of the components ) . We use the no clean > solder wire for hand soldering ,after soldering we observe that a > transparent flux residue appeared around the soldered lead and if we try to > clean it by IPA (ISO PROPYLE ALCOHALE) after drying, It will change in to > white residue and create bigger problem.After cleaning all, the surface of > PCB and solder joints get dull shining. > Pls. suggest the better way to clean > Thanks > > With regards > Pankaj Karnwal > Quality Assurance > BESL NOIDA (INDIA) > PH .91-120-4420394-5 EXTN.211 > e mail : <mailto:[log in to unmask]> > Barco, innovators in image processing > > --------------------------------------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------