Edward Yes, this is the right place to ask, but I'm not sure that I have an answer! The following is a handful of thoughts to start the debate. Ideally, all metals should be recovered for recycling. That is the easy part! As for the dust/swarf, this has been used as filler for asphalt for roads (also finely chopped laminate). The sheet material is much more controversial, mainly because of the TBBPA added to the prepolymer to render it flame retardant. I think that if it cannot be used as is (e.g. for clipboards or golf clubs), it could be landfilled provided the landfill never catches fire, releasing the bromine as hydrobromic acid. The most elegant way is incineration in an incinerator equipped with scrubbers and precipitators to eliminate all the noxious and corrosive compounds that can result. Best regards, Brian Edward Szpruch wrote: > > I believe this is the proper forum to ask the following question: > We are PCB ( bare boards ) manufacturer and of course we do have solid > wastes related to PCB: > 1) dust collected from drilling and routing operation > 2) Scrap boards and frames after routing ( epoxy+copper+tin-lead + solder > mask ) > Few days ago we had the first audit for ISO 14001 qualification. The > auditor saw one of our operators emtying collection basked full of epoxy > dust ( item 1 ) and asked how it is disposed. Today we are disposing it to > municipal waste. What is they way other are disposing it? > How the scrap boards should be disposed? > All remarks will be highly appreciated > > Edward Szpruch > Eltek Ltd > P.O.Box 159 ; 49101 Petah Tikva Israel > Tel ++972 3 9395050 , Fax ++972 3 9309581 > e-mail [log in to unmask]