For low volume production, we buy MIL approved acrylic in aerosol cans. No spray gun required. Jim Marsico Senior Engineer Production Engineering EDO Electronics Systems Group [log in to unmask] <mailto:[log in to unmask]> 631-595-5879 -----Original Message----- From: Dehoyos, Ramon [SMTP:[log in to unmask]] Sent: Tuesday, May 14, 2002 2:48 PM To: [log in to unmask] Subject: [TN] Conformal Coating My question is about conformal coating. We want to manualy conformal coat boards using a spray gun. Does anybody have knowledge of a gun that sprays pure coating without any atomization of the coating and that internally have very few parts, in case it clogs, and needs to be cleaned. Regards, Ramon ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------