How about acrylic conformal coating?
You are so far above the Tg of acrylics that the coating can "flow",
melt, evaporate, or all the above!
(Not to mention letting contaminants reach the surface!)
David A. Douthit
Manager
LoCan LLC
"Marsico, James" wrote:
Hello Technet:I think I may have asked this question a while ago (or something similar)
but couldn't find anything in the archives. I have a surface mount assembly
that gets installed into a top assembly housing, with covers. The test guys
want to subject this assembly to 125 degrees C for 112 hours. Assuming that
all of the components are rated for this temperature, is there anything else
that says this isn't a good idea? I'm thinking about the solder joints,
maybe decreased reliability due to excessive grain growth? How about
acrylic conformal coating? The PWB is polyimide, so this shouldn't be an
issue. Anything else?Thanks again...
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------