Michael, My thermal engineer assures me that the K value for copper is between 150 and 200 W/mK, but even so, your point about replacing CB100 (now CB101, by the way) with additional copper plating is a valid one, and offers much simpler, quicker and less costly PCB fabrication. The only caveat I would add is, make sure the ductility for your additional copper plating thickness is enough to avoid cracking the barrels under temperature cycling, especially if using FR4. Peter "Mcmaster, Michael" <[log in to unmask]> 26/04/2002 11:58 PM Sent by: TechNet <[log in to unmask]> Please respond to "TechNet E-Mail Forum."; Please respond to "Mcmaster, Michael" To: [log in to unmask] cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group) Subject: Re: [TN] Via Plug John The DuPont CB-100 will increase the amount of heat that can be conducted through the barrel. My experience with it that most people overestimate what it can do. I've done calculations that show for a 0.020" drilled hole with 0.001" copper barrel, adding CB-100 only increases the amount of heat by less than 5%. The reason is the CB-100 has a thermal conductivity of 5.23 W/mK vs 395 W/mK for copper. Even though CB-100 makes up the majority of the cross sectional area, it only adds a little to the "thermal" cross section. I always recommend that potential users of this technology run the numbers themselves and balance the potential cost increase with the improved performance. > ---------- > From: John Foster[SMTP:[log in to unmask]] > Reply To: TechNet E-Mail Forum.;John Foster > Sent: Tuesday, April 23, 2002 12:06 PM > To: [log in to unmask] > Subject: [TN] Via Plug > > Hello, I am new to this listserver. I must say that it is very > informative. I wish I had known of it long ago. > > I have a question about via plugging. Right now > our board vendor is doing our via plugs with > I guess with a standard epoxy. We are trying > to find a solution that would give us a much > better thermal performance. > > We are looking at silver epoxy and this > material from Dupont. Does anyone know of > some material that would give us a really good > thermal performance. We are in a commercial > environment. So the material does not have to > meet industrial specs. > > Any input on this matter would be greatly ' > appreciated. > > Thank You > > John Foster > > -------------------------------------------------------------------------- > ------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send e-mail to [log in to unmask]: > SET Technet NOMAIL > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > -------------------------------------------------------------------------- > ------- > --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- [This e-mail is confidential and may also be privileged. If you are not the intended recipient, please delete it and notify us immediately; you should not copy or use it for any purpose, nor disclose its contents to any other person. Thank you.] --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------