for a PCB with vias/thru holes
 
try 140 F with 95% RH for 96 hrs.
then reflow 3 cycles
wave solder
take a look at flow up thru holes/vias
 
some believe this represents 8 months of shelf life approx.
(from a Mike Carano IPC workshop) - thanks Mike!
 
Mike Weekes
-----Original Message-----
From: Peter Hefti [mailto:[log in to unmask]]
Sent: Thursday, April 25, 2002 2:30 AM
To: [log in to unmask]
Subject: [TN] Accelerated test for simulation of storage of PCBs with surface finish white tin


Hello TechNet:

We are searching for a method of accelerated aging of PCBs with surface finish in white tin (chemical  tin).
This method should be recognized , in order to simulate the storage of 6 or 12 month under normal conditions.
(85/85/1d or 2d  test ??)
After such an accelerated test, the solderability will be tested by the wetting balance method.

Thank you for your answer

With best regards

Peter Hefti