Earl,
What you could be seeing IMHO is the result of an
ancient technique for wave soldering called wax stabilizing. Essentially, the
through-hole components were run through a wax wave to hold them in place during
in-line lead trimming prior to entering the solder wave. Many times a joint was
contaminated and not the most reliable thing on the planet, but "it passed
test... ship it!" was the common mentality, and now you see why we don't do that
anymore. I don't think a reflow would resolve the issue at hand, since we would
still have contaminated surfaces.
Just my "dos centavos" from an old guy that
remembers stuff.
Regards,
Ed Popielarski
QTA Machine
10 Mc Laren, Ste
D
Irvine, Ca. 92618
Phone:949-581-6601
Fax: 949-581-2448
Cel:
949-337-2578