Hey Earl Where can I see these photos? Don't see them on Steve's site. Don Vischulis -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Earl Moon Sent: Friday, March 29, 2002 6:49 AM To: [log in to unmask] Subject: Re: [TN] Blistering in PCBs Vinit, Ok, here we go. Never seen nothin' like these before. Oh well, maybe once when I was a "young gun" process engineer at Xerox. That's another story I'll not bore anyone with now. Concerning the pics, it is obvious there is delam everywhere but maybe the edges. Vinitdelam3's discoloration also is delamination, not solder mask related. Someone else take shots at this and Vinit's supplier. This shop shoundn't exist unless they just lost it all on his boards ONE PING ONLY PLEASE. A pleasure to serve Vinit. Don't often get to see how bad something can be besides a train wreck. MoonMan --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------