Peter, Sounds like IPC-A-610 is exactly what you're after - fantastic document on which to "hang your hat" so to speak. Richard van Beveren NEWTRONICS PTY LTD > -----Original Message----- > From: peter lee [SMTP:[log in to unmask]] > Sent: Wednesday, 6 March 2002 18:08 > To: [log in to unmask] > Subject: [TN] Solder joint quality assessment > > Hello Technetters, > > I am conducting an independent solder joint quality > assessment on one of our customer's product. The > result of the assessment will include general > observations on overall quality of the product, visual > inspection results on all components on board > (primarily SMT), noticeable soldering defects, process > deficiencies and recommendations. > > I am looking for a formal template for my report with > a list of pass/fail criteria addressing the solder > joint quality of a product. Any advice would be > greatly appreciated. > > > __________________________________________________ > Do You Yahoo!? > Try FREE Yahoo! Mail - the world's greatest free email! > http://mail.yahoo.com/ > > -------------------------------------------------------------------------- > ------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt delivery of Technet send e-mail to [log in to unmask]: > SET Technet NOMAIL > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search previous postings at: www.ipc.org > On-Line Resources & Databases > > E-mail Archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > -------------------------------------------------------------------------- > ------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------