Where did they have the Chromatography testing done? We are looking for a facility to have this done. Thanks. Mary Jane Chism Kimball Electronics Grp -----Original Message----- From: Ted Tontis [mailto:[log in to unmask]] Sent: Friday, March 01, 2002 8:16 AM To: [log in to unmask] Subject: Re: [TN] warranty Our customer is a big named CO. and they have all ready have done the Chromatography testing and this is what they came up with. Chloride 10.5 ug/sq. in. Bromide 16.7 ug/sq. in. Some of the boards we still had sitting in shipping in there anti-static bags are showing aggressive signs of contamination. Thank you all for the information, Ted ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- -----