Flatness of board/pad finish/component. Stencil apparure design and consistent paste volume. XRay many to validate process. Pad size/ mask design/ via design. Good rework equipment. and yes Good Luck! "Crain, Bob" <[log in to unmask]> on 03/13/2002 03:44:28 PM Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to "Crain, Bob" <[log in to unmask]> To: [log in to unmask] cc: (bcc: Warren Crow/US/I-O INC) Subject: [TN] High Rel BGA Guidelines We may soon be adding BGAs to our approved parts list for some programs. We use polyamide boards and require electrical test under vibration and thermal cycling. What are the most important factors to address to maximize our success? --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------