hi, this reminds me of a situation we were in several years ago when we were using pin grid arrays. the customer required that we microsection the first, middle, and last assemblies coming out of the wave solder machine, so that we could verify that we were getting acceptable solder fillets on both sides of the pga plated-through-holes. i suggested that our lot size should be three. this would enable us to assemble these boards forever. unfortunately, no one here thought that was a good idea. what you could do is ship your assemblies with the bga's sheared off, but with the heat sinks still attached to the bga's. this would enable you to build these parts forever. i've got a feeling though that this wouldn't be acceptable, but it would get the attention of your customer. phil -----Original Message----- From: Carl Ray [mailto:[log in to unmask]] Sent: Wednesday, March 13, 2002 8:17 AM To: [log in to unmask] Subject: [TN] Solder Joint Mechanical Stress I have a customer who is requiring that I verify the bond strength of a heat sink that is glued to the top of PBGA. The customer has supplied me with a torque tool to verify the strength of the bond between the heat sink and the BGA. I have concerns that testing the strength of the glue bond may affect the solder joint reliability of the BGA. The tool supplied by the customer is set at 20 in pound torque. Any ideas how I can "change" my customer mind? --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------