We had a problem which caused our spray fluxer to kick off.  When the
panels came out of the wave, they showed definite webbing.  After they
cool down [and we fix the source of the fluxer problem], what concerns
should I have running them back through the wave with Alpha NR330 flux?


Neil Flatter
QC - Nights
TRW Automotive

---------------------------------------------------------------------------------