Hi Steve, I worked on the development of something like this a while ago. We chose pins that could 'float' by about 20 thou (mils) and the ends to be soldered were rounded. The floating allowed for coplanarity issues and the rounded ends allowed a deeper solder joint. We didn't make many but they soldered OK. By the way, the light in the tunnel is probably some blighter with a torch bringing you more work! Regards Eric Dawson > -----Original Message----- > From: [log in to unmask] [SMTP:[log in to unmask]] > Sent: Thursday, March 21, 2002 1:04 AM > To: [log in to unmask] > Subject: Re: [TN] PGA to SMT sockets... > > Hi Kerry, > > This isn't a BGA socket, but actually a Pin Grid Array (PGA) socket that > is mounted to the board to surface mount pads that looks like a BGA > footprint. This socket must be used due to the pin design that will accept > a through hole Pin Grid Array device. > > I've never seen anything like it before...got some new material for my > dreams...errr, I mean nightmares...hehehe. > > Did one experiment today trying out a few things...placed and soldered > one, it didn't look too shabby! The real test is tomorrow.... > > I think I'm seeing some light at the end of the tunnel...or is that the > headlight from the train heading towards me? > > -Steve Gregory- > > > > Hi Steve, > I would suggest you stay away from that type of socket. Try > Advanced Interconnect. Their socket has balls instead of machined pins. > Tends to work a lot better for us. > We use them when we know a die will be respinning and we want to try > a few new ones out quickly before we place a whole lot of BGA's directly > to a PCB. > As far as reflow profile......... we use the same as what the board > normally has if we are going to place say 10 - 20 of the sockets. > As far a pad size. We use the same dia pad as the ball. > We use Circuit Tech (Jeff Ferry's place) to place the socket for us > in small lots or quick turn. We also use them to mount the new BGA to the > adapter that will plug into the socket. > Hope this helps, > Kerry > > > > > --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------