When you are seeing spikes on wave solder there are a number of things to consider.

1. Is the boards being fluxed correctly and is the temperature profile correct.
2. Could the dwell time in the solder be too long.
3. If the spikes are on one component it may be worth checking the solderability.

It is unlikely that the copper content in the solder will be too high as the rate at which copper dissolves in solder reduces as the copper content increases so at normal operating temperatures it tends to be self regulating.  However, you should be doing regular checks on your solder anyway to be sure!

Regards,

Neil

Neil Atkinson




-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: 27 February 2002 23:35
Subject: Re: Solder Projections


Mr. Pollak,
High copper content in your solder can cause spikes... or amateur hand
solderers like myself are very good at forming spikes.  There may be other
reasons that some of our "older" regulars can contribute.

I looked in IPC/EIA J-STD-006 and it lists max impurity levels for different
elements, but does not give reasons why they are individually considered
impurities.  You may be able to find this info from some of the more common
reference books for our industry, the titles of which you can find by doing
a search of the TechNet archives from the IPC homepage.

regards,
Bev Christian
Research in Motion


-----Original Message-----
From: Mr. Leslie A. Pollak [mailto:[log in to unmask]]
Sent: February 27, 2002 3:57 PM
To: [log in to unmask]
Subject: [TN] Solder Projections


Hi,

Could soemone tell me what causes solder projections or what we call
icicles.

Or point us to IPC documentation that would help us.

Thanks
Mr. Leslie A. Pollak

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----


________________________________________________________________________
This e-mail has been scanned for all viruses by Star Internet. The
service is powered by MessageLabs. For more information on a proactive
anti-virus service working around the clock, around the globe, visit:
http://www.star.net.uk
________________________________________________________________________