Phil,
 
Beautiful pictures of dendritic growth.  Any other background information?
 
Hans Shin
Pacific Testing Laboratories, Inc.
www.pacifictesting.com
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of [log in to unmask]
Sent: Friday, February 22, 2002 10:50 AM
To: [log in to unmask]
Subject: Re: [TN] Dendritic Growth...

Hi Phil!

The pictures are up! Go to:

http://www.stevezeva.homstead.com

Those are the best examples of dendritic growth as I've ever seen! Where did this take place? In a SIR chamber?