Hi all,
 
 Regarding moisture sensitive devices, all the levels I see are  in respect to  <=  30c 60%RH.  The time specified for these levels are clear but what if I am dealing with 30%RH.  Is there a sliding scale that is applied to this level of humidity or do I strickly go with the times given at 60%RH.. ex. The level 5 component has 48 hours, would that be 96 hours on my production floor if I'm at 30% RH 
 
Thanks
Bob  P